Preparation of B6O Materials via Reactive and Non-Reactive Spark Plasma Sintering
25th International Baltic Conference of Engineering Materials & Tribology (Baltmattrib 2016): Abstract Book 2016
Jānis Grabis, Ints Šteins, Inta Sīpola, Dzintra Ārija Rašmane

The use of reactive spark plasma sintering of B/B2O3 at molar ratio of 14 simplified preparation technique of B6O manufacturing with relative density about 97% at 1800 oC during 5 min with respect to non-reactive sintering of B6O powder.


Keywords
Boron suboxide, reactive plasma sintering, non-reactive plasma sintering

Grabis, J., Šteins, I., Sīpola, I., Rašmane, D. Preparation of B6O Materials via Reactive and Non-Reactive Spark Plasma Sintering. In: 25th International Baltic Conference of Engineering Materials & Tribology (Baltmattrib 2016): Abstract Book, Latvia, Rīga, 3-4 November, 2016. Riga: 2016, pp.100-100. ISBN 978-9934-19-029-2.