The extraction-pyrolytic method has been applied to produce the ZnO and CdO-ZnO thin films on glass and quartz glass substrates. According to X-ray diffraction measurements, the ZnO and CdO phases have been produced with an average size of crystallites about 8–42 nm in the films. The thickness of the layers measured by a profilometer has been up to150 nm. The surface morphology measurements show that the surface of the films may be rough and non-continuous. The SEM results confirm the dependence between the preparation procedure and the quality of the thin film.


Atslēgas vārdi
CdO-ZnO thin films, extraction-pyrolytic method, surface morphology, X-ray diffraction.
DOI
10.1515/lpts-2016-0021
Hipersaite
http://www.degruyter.com/view/j/lpts.2016.53.issue-3/issue-files/lpts.2016.53.issue-3.xml

Cvetkovs, A., Kiselova, O., Rogulis, U., Serga, V., Ignatans, R. Production of ZnO AND CdO-ZnO Thin Films by Extraction–Pyrolytic Method. Latvian Journal of Physics and Technical Sciences, 2016, Vol.53, Iss.3, 57.-66.lpp. ISSN 0868-8257. Pieejams: doi:10.1515/lpts-2016-0021

Publikācijas valoda
English (en)
RTU Zinātniskā bibliotēka.
E-pasts: uzzinas@rtu.lv; Tālr: +371 28399196